Iketango eliyinhloko lamangqamuzana enayiloni 6 liqukethe amabhondi e-amide, azwelayo emisebeni ye-ultraviolet. Ngaphansi kokukhanya kwelanga kwangaphandle, ama-photon e-UV ajabulisa ukuqhekeka kwebhondi ye-amide futhi acuphe ukusabela kwama-radical mahhala, okuholela ekonakaleni kwe-polymer. Ngokwemakhroscopic, imicu ikhombisa ukuphuzi, amandla ancishisiwe okuphuka, ukuncipha kobude ngesikhathi sekhefu kanye nokwehluleka ukunqwabelana kancane kancane.
Okokukhiqiza kwezimboni zeI-I-I-I-Anti UV Filament Yarn Nylon 6, ama-stabilizers okukhanya athulwa ngesikhathi se-polymerization noma ukuphotha. Izigaba eziyinhloko zifaka izinto zokumunca ama-UV, iziqinisi ukukhanya kwe-amine ezivinjiwe (HALS) kanye nezimpushana ezivikela i-UV ezingaphili. Njengezingxenye zakwamanye amazwe zengezwe ku-PA6 matrix, izizinzisi zokukhanya zishintsha amandla e-intermolecular we-polymer. Ukulayishwa kokuqiniswa okuphezulu kuthuthukisa ukumelana nesimo sezulu se-UV, nokho umthamo oweqile wephula ukuqhubeka kwenethiwekhi ye-polymer futhi kubeke engcupheni ukuwohloka kwezakhiwo ze-fiber mechanical. Lesi yisizathu esibalulekile sokuhwebelana kokusebenza.
Izizinzisi zokukhanya zohlobo olulodwa azikwazi ukufinyelela ukumelana ne-UV isikhathi eside, ngakho-ke amasistimu ayinhlanganisela asetshenziswa kabanzi. Izibambisi ze-UV zimunca amandla e-UV kuyilapho i-HALS ithwebula ama-radicals mahhala akhiqizwa ngesikhathi sokuwohloka kwesithombe. Lezi zingxenye ezimbili zibambezela ukuguga ngendlela efanayo. Nokho, ukumelana nokushisa kuyahlukahluka phakathi kwezithasiselo. Inayiloni 6 izinga lokushisa lokuphotha ngokuvamile lisukela ku-260–280℃. Izithasiselo ezinokuzinza okunganele kokushisa ziyabola noma ziyashintshashintsha ngesikhathi sokuncibilika, zenze amabhamuza amancane ngaphakathi kokuncibilika. Lawa mabhamuza aba izindawo zokugxilisa ingcindezi kumafilaments, akhuphule izinga lokuphuka nokukhuphuka kokusatshalaliswa kwedatha ye-fiber mechanical.
Izimpushana ezingaphili njenge-titanium dioxide zivimba ngokomzimba imisebe ye-ultraviolet. Impushana ehlakazeke kahle iletha ukumelana ne-UV okuzinzile. Ngokuphambene, ama-powder agglomerate enza ukukhubazeka kwesakhiwo ngaphakathi kwemicu. Ukuqhekeka kwengcindezi kuvame ukwenzeka kulawa ma-agglomerates ngaphansi kwamandla angaphandle, okunciphisa ngokuqondile ukuqina nokuqina. Uma kuqhathaniswa neziqinisi zokukhanya kwemvelo, izigcwalisi ze-inorganic zinemiphumela emibi esobala kakhulu ekwandiseni ifayibha.
Idizayini yefomula eyinhlanganisela ibeka phambili izithasiselo ezimelana nokushisa okuphezulu ezihambisana nezimo zokuphotha ze-nylon 6. Ukusebenzisana phakathi kwe-HALS nezinqamuleli ze-UV kufinyelela ukusebenza kwesimo sezulu okuqondiwe ekulayisheni okuphelele okuphansi, kunciphisa ukuphazamiseka kusakhiwo se-PA6 samangqamuzana. Izithasiselo ezithambekele ekuguquguqukeni noma ekuboleni ekushiseni kokuphotha azifakwa ukuze kugwenywe ukonakala kwangaphakathi kumafilaments.
Uma kuqhathaniswa nokuphakelwa kwempushana okuqondile, ukuxutshwa kwe-UV masterbatch kuthuthukisa kakhulu ukufana kokuhlakazeka kwezithasiselo kuncibilika inayiloni, kuvimbele amaphuzu abuthaka endawo abangelwa ukugxila okweqile kwesengezo ezindaweni ezithile zefiber. Abathwali be-Masterbatch basebenzisa izinto ezihambisana kahle ne-PA6 matrix ukuze kuncishiswe amaphutha esixhumi esibonakalayo. Umthamo we-Masterbatch ungalungiswa ngokuya nge-filament denier kanye nohlobo lwentambo (FDY/DTY).
Ngemuva kokuqinisekiswa kwefomula, amapharamitha okuphotha athinta ukusebenza komshini kokugcina kanye nokufana kokumelana ne-UV. Izinga lokushisa elincibilikayo, i-screw back pressure kanye nokucisha izimo zomoya kuthonya ngokuqondile ukuma kwe-polymer kanye nengcindezi yangaphakathi eyinsalela. Ukulawulwa kwenqubo efanele kunciphisa ukuncibilika kwe-homogeneity, ama-bubbles nokungcola ukuze kuqinisekiswe ukwakheka okufanayo kwefayibha yangaphakathi. Ukuze uthole imicu emide ye-denier, ukunemba kwephakethe lesihlungi kuyathuthukiswa ukuze kubanjwe ama-agglomerate angahlakazeki futhi kunciphise ukuphuka kwemicu.
Imizila emibili yobuchwepheshe iyatholakalaI-I-I-I-Anti UV Filament Yarn Nylon 6: ukuguqulwa kwenqwaba kanye ne-post-finishing coating. Ukuguqulwa kwenqwaba kuhlanganisa izinzisi ekuncibilikeni ngaphambi kokuphotha. Izithasiselo zishunyekiwe phakathi kwenqwaba yefayibha, ziletha ukuwashwa okuhle nokungabambeki komhuzuko ngokusebenza okuhlala isikhathi eside kwe-UV. Nokho, ukulinganisa kwefomula kuyadingeka ukuze kugcinwe izakhiwo zemishini. I-post-finishing coating ifaka i-UV ukumelana ne-UV endaweni eqediwe yentambo. Inomthelela omncane kumakhenika wezintambo ezingavuthiwe, nokho ungqimba olungaphezulu olusebenzayo luguga kancane kancane ngemva kokungqubuzana nokuwashwa kwesikhathi eside, okuholela ekuqineni kahle kwe-UV. Ukuguqulwa kwenqwaba kuyisixazululo esijwayelekile sezinhlelo zokusebenza zangaphandle zesikhathi eside.
Ukuhlola kuphela ukwephula ukuqina kanye ne-UPF yentambo entsha akukwazi ukuhlola ngokugcwele okokusebenza. Isistimu yokuhlola ephelele ihlanganisa ukuhlolwa kokusebenza kwamasampula oqobo kanye nokuhlolwa kokuguga kwesimo sezulu esisheshayo. Ukuguga kwesibani se-Xenon kanye nokuguga kwe-QUV UV kuvame ukusetshenziswa. Izinkomba zokuhlola zihlanganisa: amandla okuqala okuphuka kanye nokwelula; izinga lokugcinwa kwamandla ngemva kokuguga, inkomba yokuphuzi kanye nezinga lokugcinwa kwe-UPF ngemva kwamahora okuguga acacisiwe.
Umbandela wokuhlola wokulinganisa okufanelekayoI-I-I-I-Anti UV Filament Yarn Nylon 6: ngemva kwemijikelezo yokuguga esheshisiwe, amafayibha asagcina amandla emishini njengoba aklanywe ngenkathi ehlangabezana nezinkomba zokuvinjwa kwe-UV okuhlosiwe. Izinga lokugcinwa kwamandla ngemva kokuguga liyinkomba eyinhloko yezimo zokusebenza zangaphandle.
Intambo ye-FDY edwetshwe ngokugcwele inama-macromolecules agxile kakhulu namandla okuqala aqinile. I-DTY draw textured thread ifaka ukunwebeka okungcono nokuthinta ngesandla okuthambile ngemva kombhalo oshisayo. Njengoba i-DTY ithunyelelwa umbhalo wezinga eliphezulu lokushisa okwengeziwe, iziqinisi ukukhanya kufomula yazo zidinga ukuzinza okuphezulu kokushisa.
Izinhlelo zokusebenza ezihlukene zidinga amaphuzu ebhalansi ahlukene. Ama-geotextiles asindayo nezintambo zibeka phambili ukugcinwa kwamandla ngemva kokuguga; izindwangu ze-shading engasindi zilinganisela ubude, i-handfeel kanye nokuvinjelwa kwe-UV okufanayo; amanethi okuvikela ezolimo ahambisana nesimo sezulu esiyisisekelo kanye nezinkomba zemishini ngaphakathi kwezinkinga zezindleko.